SECTION 900 – MATERIALS DETAILS
27.1 (20) * If the yield point of the material exceeds 450 MPa (65,000 psi), the temperature for the CVN value for acceptability shall be reduced by -10°C (15°F) for each increment of 69 MPa (10,000 psi) above 450 MPa (65,000 psi). ................
................